Molds & Tooling 7 조회수

PA6 Trapped Air Burning

문제 현상
Black spots and scorch marks at the end of the cavity, with fixed positions.
원인 분석
Poor venting diesel effect; high-speed filling at the end compresses air and heats up; PA6 processing temperature is high, and the risk of trapped air burning is large; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Open vent grooves at corresponding positions;②reduce injection speed at the filling end to leave time for venting;③clean vent grooves clogged by oil;④moderate clamping force to avoid pressing closed the parting line vent gaps;⑤reduce the amount of release agent to prevent contamination of venting.
핵심 요약
PA6 burning = 'poor venting': high-temperature nylon fears trapped air even more; opening and cleaning vent grooves is the focus of daily maintenance; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
PA6; trapped air; burning; vent grooves; diesel effect