PA6 '2079851475616104452 Yellowing
문제 현상
Natural-color PA6 turned yellow, and light transmission and appearance deteriorated.
원인 분석
Excessively high material temperature or too-long residence causes thermal oxidation; excessively high drying temperature and too-long time also cause pre-yellowing; shear heat makes the actual melt temperature exceed the standard; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Control material temperature at 240~270℃;②shorten the residence time of the melt in the barrel to reduce heat accumulation degradation;③drying temperature does not exceed 90℃;④thoroughly clean the machine to remove accumulated material in the dead corners of the barrel and hot runner;⑤reduce screw speed and back pressure to reduce shear heat generation.
핵심 요약
PA6 yellowing = 'management of heat + oxygen': check at three places of material temperature, residence, and drying temperature; nylon is sensitive to thermal oxidation, and heat history must be strictly controlled; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!