Material Drying
6 visualizaciones
PA6 '2079851475616104452 Yellowing
Fenómeno del problema
Natural-color PA6 turned yellow, and light transmission and appearance deteriorated.
Análisis de la causa
Excessively high material temperature or too-long residence causes thermal oxidation; excessively high drying temperature and too-long time also cause pre-yellowing; shear heat makes the actual melt temperature exceed the standard; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solución
①Control material temperature at 240~270℃;②shorten the residence time of the melt in the barrel to reduce heat accumulation degradation;③drying temperature does not exceed 90℃;④thoroughly clean the machine to remove accumulated material in the dead corners of the barrel and hot runner;⑤reduce screw speed and back pressure to reduce shear heat generation.
Conclusión clave
PA6 yellowing = 'management of heat + oxygen': check at three places of material temperature, residence, and drying temperature; nylon is sensitive to thermal oxidation, and heat history must be strictly controlled; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!