Processing Machinery 3 조회수

PA66 high-temperature carbonization black specks

문제 현상
Black specks on products, obvious on light-colored parts.
원인 분석
Processing above 270℃, retained material in dead corners carbonizes quickly; incomplete material changeover; high-temperature nylon has high carbonization risk; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
해결 방법
①Clean retained carbonized material in dead corners of the barrel, nozzle and hot runner; ②avoid high-temperature idle running; ③thoroughly purge during material changeover; ④establish a regular machine cleaning and maintenance system to prevent material accumulation in dead corners; ⑤check cleanliness of virgin material and regrind to eliminate contamination sources.
핵심 요약
PA66 black specks='dead corner carbonization': high-temperature nylon dead-corner material carbonizes extremely fast; machine cleaning and shutdown management must be stricter than ordinary nylon; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA66; black speck; carbonization; dead corner; material changeover