Molds & Tooling 3 조회수

PA66 nozzle drool self-locking

문제 현상
Nozzle drool stringing contaminates the mold surface, products show cold slug marks, production forced into frequent cleaning
원인 분석
PA66 melt viscosity is low; with an open nozzle, melt drools under its own weight during plasticizing back and mold opening gaps; drooled material oxidizes and enters the cavity forming cold slug marks and black specks
해결 방법
①Select self-locking (needle valve) nozzles to prevent drool; ②nozzle temperature slightly lower than the barrel front section; ③add anti-drool delayed plasticizing-back program if necessary; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PA66 processing comes standard with self-locking nozzles; eradicating drool from the hardware is more thorough and reliable than any process compensation; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PA66; drool; self-locking nozzle; needle valve; cold slug mark