Molds & Tooling 4 görüntüleme

PA66 nozzle drool self-locking

Sorun Belirtisi
Nozzle drool stringing contaminates the mold surface, products show cold slug marks, production forced into frequent cleaning
Neden Analizi
PA66 melt viscosity is low; with an open nozzle, melt drools under its own weight during plasticizing back and mold opening gaps; drooled material oxidizes and enters the cavity forming cold slug marks and black specks
Çözüm
①Select self-locking (needle valve) nozzles to prevent drool; ②nozzle temperature slightly lower than the barrel front section; ③add anti-drool delayed plasticizing-back program if necessary; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PA66 processing comes standard with self-locking nozzles; eradicating drool from the hardware is more thorough and reliable than any process compensation; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence