Material Drying
3 조회수
PBT Matte Surface Poor Gloss
문제 현상
The product surface is matte with poor gloss, and the spray-free appearance part does not meet the standard
원인 분석
PBT has excellent surface gloss performance and is suitable for spray-free applications; but too low mold temperature, insufficient resin temperature, and poor mold surface condition will cause a matte surface; spots from insufficient drying also affect gloss
해결 방법
①Increase mold temperature and resin temperature; ②Polish the mold cavity; ③Fully dry the material to prevent spots; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability
핵심 요약
PBT's spray-free advantage needs to be delivered by the process; the three elements of temperature, polishing, and drying determine surface gloss; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!