Material Drying 6 visualizações

PBT Matte Surface Poor Gloss

Fenómeno do problema
The product surface is matte with poor gloss, and the spray-free appearance part does not meet the standard
Análise das causas
PBT has excellent surface gloss performance and is suitable for spray-free applications; but too low mold temperature, insufficient resin temperature, and poor mold surface condition will cause a matte surface; spots from insufficient drying also affect gloss
Solução
①Increase mold temperature and resin temperature; ②Polish the mold cavity; ③Fully dry the material to prevent spots; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability
Conclusão principal
PBT's spray-free advantage needs to be delivered by the process; the three elements of temperature, polishing, and drying determine surface gloss; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PBT; matte surface; gloss; spray-free; mold temperature