Processing Machinery 3 조회수

PC/ABS melt temperature too high degradation

문제 현상
Parts yellow and embrittle, performance declines.
원인 분석
Polymer degrades when melt temperature exceeds 300℃; validated setpoint deviations cause internal stress and mechanical property damage.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
해결 방법
①Control melt temperature within the 240~280℃ window; ②strictly prohibit exceeding 300℃; ③calibrate the thermocouple to measure the actual melt temperature; ④shorten the residence time.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PC/ABS requires strict thermal management; 240~280℃ is the industry standard window, exceeding temperature means degradation.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PC/ABS;melt temperature;degradation;yellowing;window;calibration