Molds & Tooling 3 조회수

PCABS shrinkage rate

문제 현상
PC/ABS shrinkage rate 0.5-0.7% low, dimensional accuracy advantage.
원인 분석
PC/ABS shrinkage rate typical 0.5-0.7%; low and predictable; high-precision dimensional tolerance; complex geometry; mold design; process stability.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
해결 방법
①Design mold according to 0.5-0.7%; ②utilize dimensional accuracy; ③process stability; ④actual measurement verification; ⑤tolerance management.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PCABS low shrinkage is a dimensional accuracy advantage; mold design is precise; verification ensures accuracy.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PCABS;shrinkage rate;0.5-0.7%;dimension;precision;mold

이 정보가 도움이 되었나요?