Molds & Tooling 4 görüntüleme

PCABS shrinkage rate

Sorun Belirtisi
PC/ABS shrinkage rate 0.5-0.7% low, dimensional accuracy advantage.
Neden Analizi
PC/ABS shrinkage rate typical 0.5-0.7%; low and predictable; high-precision dimensional tolerance; complex geometry; mold design; process stability.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Çözüm
①Design mold according to 0.5-0.7%; ②utilize dimensional accuracy; ③process stability; ④actual measurement verification; ⑤tolerance management.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PCABS low shrinkage is a dimensional accuracy advantage; mold design is precise; verification ensures accuracy.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PCABS;shrinkage rate;0.5-0.7%;dimension;precision;mold

Bu faydalı oldu mu?