Injection Molding
6 조회수
PC multi-stage injection application
문제 현상
【Problem Phenomenon】PC single injection speed, jetting and shear heat coexist
원인 분석
PC multi-stage injection: slow speed at the gate to prevent jetting, medium speed in the middle section for filling, slow speed at the end section for venting and preventing burning; avoid local high shear degradation;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
Three-level or more speed curve; gate slow, middle medium, end slow; avoid high-speed shear;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability;Change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
PC multi-stage injection controls shear, slow entry, stable middle, slow finish;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!