문제 현상
The process has not changed but hazy bottles appear intermittently.
원인 분석
Dryer dew point drift, molecular sieve failure or dehumidification system failure; environmental humidity changes make the drying capacity insufficient.
해결 방법
①Dew point online monitoring and alarm; ②regular regeneration/replacement of molecular sieves; ③clean the drying filter and air duct; ④strengthen verification in high-humidity seasons.