Material Drying 5 views

PET Preform Missing Moisture Verification

Problem Phenomenon
The process has not changed but hazy bottles appear intermittently.
Cause Analysis
Dryer dew point drift, molecular sieve failure or dehumidification system failure; environmental humidity changes make the drying capacity insufficient.
Solution
①Dew point online monitoring and alarm; ②regular regeneration/replacement of molecular sieves; ③clean the drying filter and air duct; ④strengthen verification in high-humidity seasons.
Key Takeaway
Intermittent haze = drying system state drift.