문제 현상
After material change, bubbles and yellowing appear in batches; the first article was only visually inspected
원인 분석
After PET material change, drying state, melt temperature, and filtration pressure differential may all change; visual first inspection alone cannot detect hidden deviations such as IV decline and excessive moisture content
해결 방법
① Perform full-item verification of moisture content, appearance, IV or melt index, and dimensions on the first article; ② additionally measure thickness and transparency on sheet first articles; ③ mass production after parameter locking; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PET first article verification must include material state indicators; full-item verification plus parameter locking is the institutional bottom line for preventing batch accidents; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence