PPO Over-Temperature Baking and Aging
문제 현상
During PPO drying, temperature is raised or time is extended in pursuit of speed, the raw material ages, turns yellow and loses toughness, and product performance deteriorates.
원인 분석
Over-temperature and long-time baking of PPO is strictly prohibited; excessive drying causes the material to age, turn yellow and lose toughness; inaccurate temperature control of drying equipment causes local overheating; excessively thick material piles are heated unevenly.
해결 방법
①Strictly dry according to the 90~120℃×4~6 hours specification; ②calibrate the temperature control of drying equipment; ③keep material layer thickness moderate to ensure uniformity; ④downgrade yellowed material.
핵심 요약
Both insufficient and excessive PPO drying produce defects; standardized temperature and time is the only correct path; equipment temperature control accuracy needs regular calibration.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!