القائمة
المواد الآلات
رؤى
مقالات مقاطع فيديو المشاكل والحلول
About
عن Chembull شركاء الإعلام
اتصل بنا
اللغة
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
العودة إلى المشاكل والحلول
Material Drying 5 مشاهدة

PPO Over-Temperature Baking and Aging

ظاهرة المشكلة
During PPO drying, temperature is raised or time is extended in pursuit of speed, the raw material ages, turns yellow and loses toughness, and product performance deteriorates.
تحليل الأسباب
Over-temperature and long-time baking of PPO is strictly prohibited; excessive drying causes the material to age, turn yellow and lose toughness; inaccurate temperature control of drying equipment causes local overheating; excessively thick material piles are heated unevenly.
الحل
①Strictly dry according to the 90~120℃×4~6 hours specification; ②calibrate the temperature control of drying equipment; ③keep material layer thickness moderate to ensure uniformity; ④downgrade yellowed material.
الخلاصة الأساسية
Both insufficient and excessive PPO drying produce defects; standardized temperature and time is the only correct path; equipment temperature control accuracy needs regular calibration.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PPO; over-drying; aging; yellowing; toughness; baking