Molds & Tooling 4 조회수

PPS product gate design

문제 현상
Gate area defects.
원인 분석
Gate form and position affect filling and stress; PPS low viscosity gate design must be precise.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
①Optimize form and position; ②control shear; ③suitable size; ④avoid stress-bearing areas.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
Gate design affects PPS filling quality.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
PPS; gate; design; shear; filling; stress

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다