Molds & Tooling 7 visualizações

PPS product gate design

Fenómeno do problema
Gate area defects.
Análise das causas
Gate form and position affect filling and stress; PPS low viscosity gate design must be precise.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solução
①Optimize form and position; ②control shear; ③suitable size; ④avoid stress-bearing areas.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Gate design affects PPS filling quality.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
PPS; gate; design; shear; filling; stress