PPS Full Regrind Feasibility

문제 현상
Attempting high-ratio regrind production, strength retention is unexpectedly good but appearance declines
원인 분석
Research shows that after 7 recycling cycles, PPS regrind still retains about 85% of its mechanical properties, and its thermal stability is better than most engineering plastics; but appearance and color deteriorate cycle by cycle, and parts with high appearance requirements still need restricted use
해결 방법
①The regrind ratio can be relaxed for internal structural parts; ②Appearance parts are still controlled at 25-30%; ③Record cycle counts and conduct performance sampling; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
PPS's regrind tolerance stands out among engineering plastics; the 85% retention rate gives large reuse room for internal parts; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PPS; full regrind; 85%; thermal stability; recycling