Injection Molding 5 조회수

PVC Weld Line and Flow Mark

문제 현상
Weld lines and flow marks on products were obvious; raising temperature gave limited improvement and approached degradation
원인 분석
When PVC melt temperature is low, poor front convergence forms weld lines; but temperature-raising room is limited by degradation, so it mainly relies on injection speed and gate position optimization; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
해결 방법
①Adjust injection speed to improve front convergence; ②optimize gate position to adjust weld line position; ③moderately raise mold temperature when necessary; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PVC weld line treatment mainly relies on speed and position; use temperature means cautiously and strictly prevent crossing into degradation; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PVC;weld line;flow mark;injection speed;gate