Injection Molding
6 görüntüleme
PVC Weld Line and Flow Mark
Sorun Belirtisi
Weld lines and flow marks on products were obvious; raising temperature gave limited improvement and approached degradation
Neden Analizi
When PVC melt temperature is low, poor front convergence forms weld lines; but temperature-raising room is limited by degradation, so it mainly relies on injection speed and gate position optimization; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Çözüm
①Adjust injection speed to improve front convergence; ②optimize gate position to adjust weld line position; ③moderately raise mold temperature when necessary; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
PVC weld line treatment mainly relies on speed and position; use temperature means cautiously and strictly prevent crossing into degradation; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu