Warpage in PU '2079851475616104452
문제 현상
PU injection molded products warp 2-3mm/100mm after demolding, flatness not up to standard
원인 분석
PU shrinkage large and mold temperature uneven causing shrinkage differences in each direction; gate location improper, flow orientation stress unevenly released; cooling time insufficient
해결 방법
1) Increase mold temperature to 40-60°C to reduce temperature difference; 2) Increase holding pressure 50-70MPa; 3) Optimize gate location for uniform flow; 4) Extend cooling time; 5) Annealing to release residual stress
핵심 요약
Warpage is caused by shrinkage differences and orientation stress; uniform mold temperature and holding are key