Molding Process
7 조회수
PU Extruded Film Thick Edges and Thin Middle
문제 현상
PU extruded film edges 20-30% thicker than the middle, thickness in U-shaped distribution
원인 분석
Die flow channel design improper, edge resistance low and flow large; PU melt elasticity, swell larger at edges; air ring cooling edge effect different
해결 방법
1) Die with coat-hanger design to balance middle and edge resistance; 2) Fine-tune die gap slightly larger in the middle and slightly smaller at the edges for compensation; 3) Slightly reduce air volume at the air ring edges; 4) Add restrictor bar to adjust edge flow
핵심 요약
U-shaped thickness is caused by die flow channel and swell differences; coat-hanger die and gap fine-tuning are key
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다