Injection Molding
5 조회수
PVA injection cold slug marks
문제 현상
PVA injection molded product shows cold slug marks near the gate
원인 분석
Nozzle temperature on the low side causes residual material from the previous shot to cool and solidify in the nozzle; cold slug well design insufficient to accommodate the cold slug; injection pressure insufficient
해결 방법
1) Raise nozzle temperature to 140-200°C; 2) Mold design with a sufficiently large cold slug well; 3) Ensure fresh melt at the nozzle front before each injection; 4) Increase injection pressure to push the cold slug through the gate
핵심 요약
Cold slug marks are caused by solidified residual material in the nozzle; raising nozzle temperature and cold slug well design are the key
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!