PVA internal shrinkage voids
문제 현상
PVA thick-wall product center shrinkage voids diameter 0.5-2mm
원인 분석
After cooling of the thick-wall area, the interior shrinks but the surface has solidified and cannot be fed; holding time insufficient, gate freezes too early
해결 방법
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness differences
핵심 요약
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is the key