Molds & Tooling 3 Aufrufe

PVA internal shrinkage voids

Problembeschreibung
PVA thick-wall product center shrinkage voids diameter 0.5-2mm
Ursachenanalyse
After cooling of the thick-wall area, the interior shrinks but the surface has solidified and cannot be fed; holding time insufficient, gate freezes too early
Lösung
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness differences
Wichtigste Erkenntnis
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is the key
PVAshrinkage voidthick wallholding timegate freezing