Wall thickness >5mm thick-walled products have prominent sink marks and bubble problems

문제 현상
Wall thickness >5mm thick-walled products have prominent sink marks and bubble problems
원인 분석
Thick walls have long cooling time, internal cooling slow, outer layer solidifies first, internal shrinkage sink marks Holding pressure time insufficient, thick wall center not compacted Gate too small, holding pressure cannot be transmitted to the thick wall center Bubbles and voids inside thick walls Cellulose acetate butyrate shrinkage rate 0.4-0.6%, thick wall shrinkage more obvious
해결 방법
Extend holding pressure time to ensure thick walls are fully compensated for shrinkage Increase gate size, extend gate freezing time Lower the mold temperature to accelerate outer layer cooling of thick walls Extend overall cooling time Avoid excessively thick wall thickness in design
핵심 요약
Thick walls require extended holding pressure and cooling time
thick-wall injectionextended holding pressuresink markcooling