Wall thickness >5mm thick-walled products have prominent sink marks and bubble problems

Fenómeno del problema
Wall thickness >5mm thick-walled products have prominent sink marks and bubble problems
Análisis de la causa
Thick walls have long cooling time, internal cooling slow, outer layer solidifies first, internal shrinkage sink marks Holding pressure time insufficient, thick wall center not compacted Gate too small, holding pressure cannot be transmitted to the thick wall center Bubbles and voids inside thick walls Cellulose acetate butyrate shrinkage rate 0.4-0.6%, thick wall shrinkage more obvious
Solución
Extend holding pressure time to ensure thick walls are fully compensated for shrinkage Increase gate size, extend gate freezing time Lower the mold temperature to accelerate outer layer cooling of thick walls Extend overall cooling time Avoid excessively thick wall thickness in design
Conclusión clave
Thick walls require extended holding pressure and cooling time
thick-wall injectionextended holding pressuresink markcooling