Injection Molding 5 조회수

CEF and color masterbatch mixing color uneven

문제 현상
The CEF/color masterbatch injection molded part shows color streaks and areas with uneven color depth
원인 분석
The carrier resin of the color masterbatch is incompatible with CEF; the color masterbatch is poorly dispersed and the pigment agglomerates; the melt flow is unstable during the '2079851475616104452 process, causing pigment orientation
해결 방법
1) Select CEF or similar carrier color masterbatch to ensure compatibility; 2) Pre-disperse by twin-screw extrusion granulation; 3) Appropriately extend the mixing time to ensure pigment dispersion; 4) Reduce the injection speed to reduce pigment orientation
핵심 요약
Carrier matching of the color masterbatch and sufficient dispersion are the key to color uniformity
CEF coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streak