Injection Molding 2 visualizaciones

CEF and color masterbatch mixing color uneven

Fenómeno del problema
The CEF/color masterbatch injection molded part shows color streaks and areas with uneven color depth
Análisis de la causa
The carrier resin of the color masterbatch is incompatible with CEF; the color masterbatch is poorly dispersed and the pigment agglomerates; the melt flow is unstable during the '2079851475616104452 process, causing pigment orientation
Solución
1) Select CEF or similar carrier color masterbatch to ensure compatibility; 2) Pre-disperse by twin-screw extrusion granulation; 3) Appropriately extend the mixing time to ensure pigment dispersion; 4) Reduce the injection speed to reduce pigment orientation
Conclusión clave
Carrier matching of the color masterbatch and sufficient dispersion are the key to color uniformity
CEF coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streak

¿Le ha resultado útil?