CEF material changeover residue
문제 현상
After CEF material changeover, the first 5-10 products contain the previous raw material residue, color difference and performance deviation
원인 분석
The previous raw material residue in the barrel and screw is large; the cleaning is not thorough and there is residue in the dead corner area; the cleaning material amount is insufficient
해결 방법
1) Increase the cleaning material amount to 2-3 times the barrel capacity; 2) Increase the speed and temperature during cleaning to accelerate removal; 3) Disassemble the screw to thoroughly clean the dead corners
핵심 요약
Material changeover residue is caused by incomplete cleaning; sufficient cleaning and disassembly are the key