Processing Machinery 8 visualizaciones

CEF material changeover residue

Fenómeno del problema
After CEF material changeover, the first 5-10 products contain the previous raw material residue, color difference and performance deviation
Análisis de la causa
The previous raw material residue in the barrel and screw is large; the cleaning is not thorough and there is residue in the dead corner area; the cleaning material amount is insufficient
Solución
1) Increase the cleaning material amount to 2-3 times the barrel capacity; 2) Increase the speed and temperature during cleaning to accelerate removal; 3) Disassemble the screw to thoroughly clean the dead corners
Conclusión clave
Material changeover residue is caused by incomplete cleaning; sufficient cleaning and disassembly are the key
CEFmaterial changeover residuecleaning materialscrew disassemblydead corner cleaning