MP large dimensional change with temperature
문제 현상
MP product dimensions change >2% in the -20 to 60°C range
원인 분석
MP thermal expansion coefficient large; crystallinity low causing high dimensional temperature sensitivity; not annealed, residual stress present
해결 방법
1) add rigid filler to lower the thermal expansion coefficient; 2) annealing to stabilize dimensions; 3) select a high crystallinity grade to reduce temperature sensitivity
핵심 요약
dimensional temperature sensitivity is caused by large thermal expansion coefficient; adding filler and annealing are key