Extrusion & Post 8 views

MP large dimensional change with temperature

Problem Phenomenon
MP product dimensions change >2% in the -20 to 60°C range
Cause Analysis
MP thermal expansion coefficient large; crystallinity low causing high dimensional temperature sensitivity; not annealed, residual stress present
Solution
1) add rigid filler to lower the thermal expansion coefficient; 2) annealing to stabilize dimensions; 3) select a high crystallinity grade to reduce temperature sensitivity
Key Takeaway
dimensional temperature sensitivity is caused by large thermal expansion coefficient; adding filler and annealing are key
MP dimensional temperature sensitivity thermal expansion coefficient rigid filler annealing