Injection Molding 4 조회수

Solution for mildew-proof treatment of calcium-zinc stabilizer in injection nozzle scorching

문제 현상
The calcium-zinc PVC system shows mildew-proof treatment-related abnormalities in the injection nozzle scorching production stage, production capacity is limited.
원인 분석
The initial coloring characteristic of calcium-zinc stabilizers produces mildew-proof treatment problems under specific working conditions.
해결 방법
From the formulation perspective, increase auxiliary stabilizers, combined with process optimization to solve it.
핵심 요약
The mildew-proof treatment problem of the calcium-zinc system in the injection nozzle scorching stage requires bidirectional adjustment of formulation and process.