Injection Molding
7 visualizações
Solution for mildew-proof treatment of calcium-zinc stabilizer in injection nozzle scorching
Fenómeno do problema
The calcium-zinc PVC system shows mildew-proof treatment-related abnormalities in the injection nozzle scorching production stage, production capacity is limited.
Análise das causas
The initial coloring characteristic of calcium-zinc stabilizers produces mildew-proof treatment problems under specific working conditions.
Solução
From the formulation perspective, increase auxiliary stabilizers, combined with process optimization to solve it.
Conclusão principal
The mildew-proof treatment problem of the calcium-zinc system in the injection nozzle scorching stage requires bidirectional adjustment of formulation and process.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!