Material Drying
4 조회수
Control of viscosity abnormality in PEOX extrusion laundry pods
문제 현상
During PEOX extrusion production of laundry pods, the problem of not up to standard viscosity occurs.
원인 분석
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and shear heat accumulation.
해결 방법
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
핵심 요약
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.