Control of viscosity abnormality in PEOX extrusion laundry pods
Fenómeno do problema
During PEOX extrusion production of laundry pods, the problem of not up to standard viscosity occurs.
Análise das causas
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and shear heat accumulation.
Solução
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Conclusão principal
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.