문제 현상
During PEOX coating production of water-soluble bags, the problem of uneven viscosity occurs.
원인 분석
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
해결 방법
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
핵심 요약
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.