Material Drying
2 views
Control of viscosity abnormality in PEOX coating water-soluble bags
Problem Phenomenon
During PEOX coating production of water-soluble bags, the problem of uneven viscosity occurs.
Cause Analysis
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
Solution
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Key Takeaway
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
Was this helpful?
0 people found this helpful
Thank you for your feedback!