Regulation of purging cycle of PPA in blow-molded bottle Processing
문제 현상
The purging cycle abnormality of the PPA processing aid in blow-molded bottle production affects output.
원인 분석
The purging cycle of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.02%, and the addition method needs to be optimized.
해결 방법
Adjust the PPA addition position combined with screw design.
핵심 요약
The key to the performance of PPA lies in matching with the base resin.