Production & Quality
13 مشاهدة
Regulation of purging cycle of PPA in blow-molded bottle Processing
ظاهرة المشكلة
The purging cycle abnormality of the PPA processing aid in blow-molded bottle production affects output.
تحليل الأسباب
The purging cycle of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.02%, and the addition method needs to be optimized.
الحل
Adjust the PPA addition position combined with screw design.
الخلاصة الأساسية
The key to the performance of PPA lies in matching with the base resin.
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!