PC/ABS heat deflection temperature insufficient
문제 현상
PC/ABS HDT does not meet heat resistance requirements (e.g., automotive interior 80-110°C).
원인 분석
PC/ABS HDT depends on PC content and processing conditions; HDT is about 100-120°C.
해결 방법
Increase PC content; full annealing (80-100°C/2h) to increase HDT.
핵심 요약
PC/ABS heat resistance can be improved through formulation and annealing.