Injection Molding
4 조회수
Abnormal injection melt viscosity
문제 현상
The melt flows with difficulty, the injection pressure is high, and the filling is incomplete
원인 분석
Temperature <210C causes insufficient plasticization, or >270C causes crosslinking
해결 방법
Strict 220-260C segmented temperature control, empty the material after a 10min shutdown
핵심 요약
The processing temperature window is narrow and the operation requirements are high