Injection Molding
5 görüntüleme
Abnormal injection melt viscosity
Sorun Belirtisi
The melt flows with difficulty, the injection pressure is high, and the filling is incomplete
Neden Analizi
Temperature <210C causes insufficient plasticization, or >270C causes crosslinking
Çözüm
Strict 220-260C segmented temperature control, empty the material after a 10min shutdown
Temel Çıkarım
The processing temperature window is narrow and the operation requirements are high
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu