Extrusion & Post
4 조회수
Metallocene linear low density polyethylene film gel particles/gel granules
문제 현상
Transparent or translucent granular gel particles are visible in the film, affecting film appearance and transparency.
Gel particles are insufficiently plasticized resin or crosslinked gel, especially obvious in transparent films.
원인 분석
(1) The high molecular weight fraction in the raw material is not fully plasticized\
(2) Extrusion temperature too low\
(3) Insufficient screw mixing effect\
(4) The raw material contains crosslinked gel\
(5) The filter screen mesh count is insufficient
해결 방법
(1) Increase extrusion temperature to the higher value within the 190-260°C range\
(2) Optimize screw design, add mixing elements\
(3) Select high-quality raw material with low gel content\
(4) Increase the filter screen mesh count to 80-120 mesh\
(5) Regularly clean the screw and die to prevent carbide formation
핵심 요약
Gel particles are caused by insufficient plasticization or raw material quality problems, and need to be solved from temperature control and raw material quality.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!