Heat extension of cross-linked polyethylene XLPE products exceeding the standard

문제 현상
The elongation of XLPE products in the heat extension test exceeds the limit of 175%. Heat extension exceeding the standard indicates insufficient cross-linking degree or incomplete cross-linking network, and the product is easily deformed at high temperatures.
원인 분석
(1)The cross-linking degree is insufficient and the cross-linking network density is not enough (2)The cross-linking temperature is too low or the time is insufficient (3)The peroxide dosage is insufficient (4)The silane cross-linking condensation is incomplete (5)The irradiation cross-linking dose is not enough
해결 방법
(1)Increase the cross-linking agent dosage to the optimized formulation value (2)Raise the cross-linking temperature or extend the cross-linking time (3)Check the catalyst activity and warm water cross-linking conditions (4)Increase the dose for irradiation cross-linking or perform post-treatment annealing (5)Regularly test the heat extension index and establish quality control records
핵심 요약
Heat extension exceeding the standard is a direct manifestation of insufficient cross-linking degree, and needs to be comprehensively adjusted from the cross-linking formulation and process parameters.
heat extensioncross-linking degreecross-linking agent dosagecross-linking temperaturecross-linking network