PETG '2079851475616104452 screw speed too high, gasification
문제 현상
Excessive screw speed causes melt shear overheating, bubbles and degradation.
원인 분석
Excessive screw speed produces a large amount of shear heat, exceeding the PETG thermal stability limit.
해결 방법
Reduce the screw speed to a reasonable range of 50-100rpm; use back pressure to discharge gas.
핵심 요약
PETG screw speed should be as low as possible under the premise of ensuring plasticization.