Material Analysis
4 조회수
Substandard Weather Resistance of Modified Acrylate-Epoxy-Phosphate-Distyrene Copolymer
문제 현상
The weather resistance of modified acrylate-epoxy-phosphate-distyrene copolymer is substandard, and after outdoor use, yellowing, embrittlement, or significant performance decline occurs
원인 분석
No ultraviolet absorber is added or the addition amount is insufficient
The antioxidant system is imperfect
The ultraviolet absorber has poor compatibility with the acrylate-epoxy-phosphate-distyrene copolymer
The antioxidant is consumed and degraded during processing
The formulation design is unreasonable
해결 방법
Add an appropriate amount of ultraviolet absorber (0.2-0.5%)
Improve the antioxidant system with the combination of primary/secondary antioxidants
Select a UV absorber with good compatibility
Avoid high-temperature degradation of antioxidants during processing
Optimize the formulation design
핵심 요약
Weather resistance needs to be addressed from UV absorbers and antioxidants